extrusion die
metal die
1.Long history
2.Using advanced software
3.Delivery on time
4.Heat treatment
metal die
1. Over 18 years of die manufacture experiences, and also several years OEM experiences.
2. Using advanced software: CAD, CAXA, SOLIDWORD, SBDS.
3. Reasonable production plan
4. Processing with advanced production system.
5. Suitable carbon or wooden box packing
6. Practical usage and good durability.
7. Delivery on time.
8. Heat treatment:
Quench:1000-1040`C via 600`C and 850`C, preheating oil or wind cooling
Temper temperature and rigidity HBC(reference) quench
hardening 108-300`C 450-500`C 550-5700`C
53-55 51-52 53-54 50-52
Temper temperature should be higher than working temperature in order to stabilize the
working size of mold.
Heat up to 650`C of average temperature in order to eliminate themachined stress, 500` air cooling after electric cooker cooling
Tempering, 800-850`C,slow cooling after diathermia.